Passenger's Side Rust This the sub frame under the rear passenger's seat. It looks pretty bad.
Passenger's Side Rust This is the same area on the driver's side no rust at all.
Passenger's Side Rust Started removing the outer subframe to reveal a thinner box under it. The outer subframe is 12 gauge and the inner box is 16 gauge.
Passenger's Side Rust The previous shot was too dark and this shot is too bright. You get ther point, rotten metal is gone, some pitted metal remains, a little more cutting to do, and then prep for patches.
Passenger's Side Rust From the bottom you can see the one spot weld was holding pretty good, the small hole between the two larger holes.
Passenger's Side Rust This is the wheel well that caps the rocker panel.
Passenger's Side Rust Another shot of the wheel well capping off the rocker panel and the door jamb area of the quarter panel.
Passenger's Side Rust This is where the quarter panel meets the rocker panel.
Passenger's Side Rust Part of the inner door jamb brace is gone and the last 6 inches of the rocker panel is badly rusted.
Passenger's Side Rust Small section of the door jamb skin will need some rust repair too.
Passenger's Side Rust Rear of wheel well opening. This is one of two spots with rot. I might just patch this side instead of replacing the entire wheel well and quarter panel skin.
Passenger's Side Rust Front of the rear wheel well rot. Two patches or the whole skin???